jilly
off to a rocking start
Member since November 2010
Posts: 17
|
Post by jilly on Dec 17, 2010 16:01:43 GMT -5
I have some spectrolite for tumbling. The pieces are sort of smallish and I don't want to lose too much off them, but I do want the rough edges smoothed out. Suggestions? I thought of tumbling them for a few days in 220 grit, then switching them over to the vibe.
|
|
|
Post by tntmom on Dec 23, 2010 19:53:37 GMT -5
bump...
I've read somewhere that spectrolite should never go in a rotary and is only partially successful in a vibe. I personally have never tried tumbling it. I have some though.... will follow this post for expert advice!
|
|