I am about ready for a 500 aluminum oxide pre-polish on an agate batch, I have some 600 silicon carbide i want to use up, will the 600 SC act about equally as the 500 AO on the agate? or would that be a mistake? TIA
|
|
|
Post by jakesrocks on Sept 7, 2011 9:34:28 GMT -5
I always use 600 SC, and have had no problems with it.
|
|
charles kuchar
spending too much on rocks
getting ready for the second coming
Member since November 2010
Posts: 300
|
Post by charles kuchar on Sept 7, 2011 21:15:54 GMT -5
i use 1/2 t of ao500 and 1/2 t of sic 500 in my last phase in the vibe before i start the polish phase. seems to work real good together. charlie
|
|
|
Post by susand24224 on Sept 8, 2011 21:42:22 GMT -5
Ditto what Jakesrocks said. I've not been real impressed with "straight" AO as a grit although I've never mixed it with Sic.